Additive of copper plating machine for gravure cylinder making

Product name:Additive for copper plating machine

1.For brightness

2.For hardness

Gravure Engraving acid copper plating additive
(hard, filled type)
Features:
1. Japanese formula of production, hardness can endure;
2. most suitable for engraving or e-corrosion plate;
3. filled capacity significantly improved, with an appropriate degree of scalability;
4. do not have a crystal tree, Ma, Au, such as stuffing;
5. can conduct high-current electroplating;
6. of the mixed reaction is not sensitive;
7. compatible with other additives to import or domestic;
25kg plastic barrels packaging, non-dangerous goods should be stored in a closed-Indoor!
Electroplating process:
Raw material standards
Bluestone 200-240g / L
Sulfate 50-70g / L
Cl- 100-150mg / L
LK - 1 1.5-3ml / L
LK - 2 1.5-3ml / L
Temperature 38-41 ℃
Cathode current density 15-20A/dm2

Additives added methods and amp hours, the current method of calculation :
1.LK-1 added volume of 80-120 ml / 1,000 amp hours;
LK - 2 additional volume 80-120 ml / 1,000 amp hours;
2. Electrolysis capacity (ampere hours) = set thickness (mm) × diameter (mm) × 3.14 × long (mm) × 0.00717
3. The current (amps) = cathode current density × diameter (mm) × 3.14 × long (mm) × 0.0001
4. Electroplating time (minutes) = electrolysis capacity (ampere hours) × 60 / total current (amps)

Correction of fauits


Nature of defect

Possible cause

Treeings burnt deposit on edges

1.Low temperature

2.Excessive current density

3.Deficiency of metal or acid

4.Excess of LK-1

5.Deficiency of LK-2

6.Lack of anodes

7.Insufficient shield

Streaks on edges in extreme cases like a screw

1.Deficiency of chlorine ion

Weak brightness Mat deposit or streaks in the middle area

1.High temperature

2.Slow rate of deposition

3.Excess of LK-2

4.Deficiency of LK-1

5.Deficiency of acid

Rough granular or pitted deposit linear dented flaws

1.Insufficient grinding on the substrate

2.Insufficient filtration

3.Insufficient pretreatment

4.Insufficient strike

5.Ironic Contamination

6.Organic contamination

7.Insufficient quality of anodes

8.Excess of metal or acid

9.Falling of dust from carrier,hoist

10.Sons in upper tank

11.Insufficient Ballard

12.Excess off chlorine ion(granular deposit on high current density areas)

Deposit very hard in extreme cases brittle

1.Excess of LK-1

2.Deficiency of LK-2

Deposit too soft hardness changes in the time

1.Deficiency of LK-1

2.Excess of LK-2

Thickness is in-homogeneous or undulation

1. Insufficient arrangement of anode baskets

2.Lack of anodes

Current falls after the bath has been in use

1.Excess of metai

2.Extraordinary excess of chlorine ion

3.Lack of anodes

4.Low temperature

5.Insufficient circuits

Kindly sent us your comsumable usual required specific request list with needed quantity,we will sent our offer for your consideration in toghether.

Quality Additive of copper plating machine for gravure cylinder making for sale
Send your message to this supplier
 
From:
To: YUBO Gravure Cylinder Making Machinery
Subject:
Message:
Characters Remaining: (0/3000)
 
You may also be interested in :
Inquiry Cart 0
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
  • Submit Buying Request
    Contact Us Quickly