Categories | Nickel Alloy Rod |
---|---|
Brand Name: | Zhonggong Special Metallurgy |
Model Number: | GH32 Alloy |
Place of Origin: | China |
MOQ: | 100KG |
Price: | Price is negotiated based on the required specifications and quantity |
Payment Terms: | Payment Terms: Mainly T/T.. L/C, D/A, D/P, |
Supply Ability: | 5000 tons per month |
Delivery Time: | 5-8 working days, depending on the parameters required for negotiation |
Packaging Details: | Standard export packaging, or packaging as required |
Certification: | ISO Certificate |
GH32 Alloy is a high-performance nickel-based superalloy designed for demanding high-temperature applications. Known for its superior mechanical properties, GH32 offers exceptional strength, excellent oxidation resistance, and outstanding corrosion resistance. The alloy's composition typically includes nickel, chromium, cobalt, molybdenum, and other elements to enhance its durability and stability at elevated temperatures.
GH32 Alloy is utilized in applications where high strength, temperature stability, and resistance to harsh conditions are essential. Its advanced properties ensure reliable performance in some of the most challenging industrial and aerospace environments.
Here’s a detailed composition table for GH32 Alloy:
Element | Composition (%) |
---|---|
Nickel (Ni) | Balance |
Chromium (Cr) | 19.0 - 21.0 |
Cobalt (Co) | 10.0 - 12.0 |
Molybdenum (Mo) | 2.0 - 4.0 |
Titanium (Ti) | 2.0 - 2.5 |
Aluminum (Al) | 1.0 - 1.5 |
Carbon (C) | ≤ 0.08 |
Silicon (Si) | ≤ 0.50 |
Manganese (Mn) | ≤ 0.50 |
Boron (B) | ≤ 0.01 |
These values provide a general guideline, but specific alloy grades may have slight variations based on the manufacturer's standards and requirements.
![]() |